AWS tasnifi: AWS 5.9
TA'RIF:
Zanglamaydigan po'latdan yasalgan payvandlash simlari yuqori qoplama samaradorligiga ega, barcha pozitsiyalarda payvandlashda yaxshi payvandlash texnik ko'rsatkichlariga ega. Ular sanoatda keng qo'llaniladi: qurilish inshootlari, transport vositalari, ko'prik muhandisligi, konchilik mashinalari, temir yo'l, neft quvurlari, gaz bosimi ko'taruvchi uskunalar, quvvat uskunalari va boshqalar.
MODEL RAQAMI VA O'LCHAMI:
1. Zavod ta'minoti OEM xizmati.
2. Model: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi va boshqalar.
3. MIG simining o'lchami: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4.TIG simining o'lchami: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
KIRISH:
Biz turli xil zanglamaydigan po'latdan yasalgan payvandlash simlarini, jumladan, Mig qattiq payvandlash simini, Tig novda payvandlash simini va suv osti yoyli payvandlash simlarini taqdim etamiz, ularning barchasi yuqori sifatli va butun dunyo bo'ylab sotiladi.
308 va 309 dan tashqari, biz 304, 321, 347, 316L, 310, 2209 va 201 ni ham taklif etamiz. Shuningdek, 318L, 904L, 2594, NiCrMo-3, Ni1 kabi maxsus texnik xususiyatlar ham mavjud.
QADOQLASH:
Mig payvandlash simlarini o'rash (g'altak va baraban to'plami)
Diametri: 0,8 - 2,0 mm
Paket: 1 kg/g'altak, 5 kg/g'altak, 15 kg/g'altak, 20 kg/g'altak, 100 kg/baraban, 200 kg/baraban
Tig rodli payvandlash simlarini o'rash (plastik naycha)
Diametri: 1.0 - 5.0 mm
Paket: 5 kg/paket
Suv osti yoyli payvandlash simi
Diametri: 2,5 - 5,0 mm
Paket: 20 kg/paket, 25 kg/paket
Neytral qadoqlash va OEM xush kelibsiz!
ZANGLAMASLIK PO'LATDAN YANGILGAN PAYVANDLASH SIMINING KIMYOVIY TARKIBI:
| Model raqami | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0,045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0,003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0,045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0,5-1,5 | 0,75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0,75 | 0,75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0,75 | 0,75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0,75 | 0,75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0,75 | 0,75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0,75 | 0,75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0,75 | 0,75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0,75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0,75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0,75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0,75 | 0,75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0,75 | 0,75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0,75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0,75 | 0,75 |
| Model raqami | Cho'zilish kuchi Rm (Mpa) | Hosildorlik kuchi Rel yoki Rp0.2 (Mpa) | Uzayish (%) | Model raqami | Cho'zilish kuchi Rm (Mpa) | Hosildorlik kuchi Rel yoki Rp0.2 (Mpa) | Uzayish (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| TIG va MIG zanglamaydigan po'latdan yasalgan payvandlash simlarining tarkibi | ||||||||||
| YB5092-2005 | AWS | Kimyoviy tarkibi % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0,022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0,045 | 0.45 | 1.9 | 0.02 | 0,009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0,006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0,045 | 0.85 | 1.5 | 0,022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0,009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0,009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0,022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0,05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0,022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0,022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0,022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0,022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0,055 | 0.48 | 1.8 | 0.021 | 0,008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0,5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0,022 | 0,5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0,5 | 1 | 0,025 | 0,015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0,022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mo | 0,023 | 0.45 | 1.5 | 0,022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0,5 | 0,022 | 0.01 | 16.5 | 4.8 | Cu;3 Nb;0.28 | |
| H08Cr26Ni5Mo2 | ER453lar | 0.06 | 0.3 | 0.4 | 0,022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0,35 | 5.5 | 0,022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0,022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
Wenzhou Tianyu Electronic Co., Ltd. 2000-yilda tashkil etilgan. Biz 20 yildan ortiq vaqt davomida payvandlash elektrodlari, payvandlash tayoqchalari va payvandlash materiallari ishlab chiqarish bilan shug'ullanib kelmoqdamiz.
Bizning asosiy mahsulotlarimiz zanglamaydigan po'latdan payvandlash elektrodlari, uglerodli po'latdan payvandlash elektrodlari, past qotishmali payvandlash elektrodlari, sirt payvandlash elektrodlari, nikel va kobalt qotishmali payvandlash elektrodlari, yumshoq po'lat va past qotishmali payvandlash simlari, zanglamaydigan po'latdan payvandlash simlari, gaz bilan himoyalangan flyusli o'zakli simlar, alyuminiy payvandlash simlari, suv osti yoyli payvandlash, simlar, nikel va kobalt qotishmali payvandlash simlari, jez payvandlash simlari, TIG va MIG payvandlash simlari, volfram elektrodlari, uglerodli payvandlash elektrodlari va boshqa payvandlash aksessuarlari va sarf materiallarini o'z ichiga oladi.
Wenzhou Tianyu Electronic Co., Ltd. 2000-yilda tashkil etilgan. Biz 20 yildan ortiq vaqt davomida payvandlash elektrodlari, payvandlash tayoqchalari va payvandlash materiallari ishlab chiqarish bilan shug'ullanib kelmoqdamiz.
Bizning asosiy mahsulotlarimiz zanglamaydigan po'latdan payvandlash elektrodlari, uglerodli po'latdan payvandlash elektrodlari, past qotishmali payvandlash elektrodlari, sirt payvandlash elektrodlari, nikel va kobalt qotishmali payvandlash elektrodlari, yumshoq po'lat va past qotishmali payvandlash simlari, zanglamaydigan po'latdan payvandlash simlari, gaz bilan himoyalangan flyusli o'zakli simlar, alyuminiy payvandlash simlari, suv osti yoyli payvandlash, simlar, nikel va kobalt qotishmali payvandlash simlari, jez payvandlash simlari, TIG va MIG payvandlash simlari, volfram elektrodlari, uglerodli payvandlash elektrodlari va boshqa payvandlash aksessuarlari va sarf materiallarini o'z ichiga oladi.